Muriatic acid as a cleaner of kiln wash

Muriatic acid is a common name for hydrochloric acid.   Let’s look at what is being cleaned off first.

The main components of kiln wash are hydrated aluminia, kaolin, and colouring. Colouring burns away, hydrated aluminum is inert at kilnforming temperatures, Kaolin begins a non-reversable change from hexagonal plates to a crystalline form at about 600C/1100F and completes it by 900C/1650F. Now consider the characteristics of each element. 

Aluminium Oxide

Aluminium oxide is widely used for its hardness and strength. It is only slightly softer than diamond. In its hydrated form it is a separator between glass and supporting structures. It has excellent refractory characteristics with a melting point of 2,072 °C/3,762 °F. But it is insoluble in water and all solvents. It is largely impervious to acids. 

Kaolin


Kaolinite structure, showing the interlayer hydrogen bonds in white.
Source: Wikipedia
 

Compared with other clay minerals, kaolinite is chemically and structurally simple. It consists of layers, each bound together by shared oxygen ions. The layers are bonded via hydrogen bonding between oxygen on the outer face of one sheet and the other. … The close hydrogen bonding between layers also hinders water molecules from infiltrating between layers, accounting for kaolinite's non-swelling character.

When moistened, the tiny plate-like crystals of kaolinite acquire a layer of water molecules that cause crystals to adhere to each other and give kaolin clay its cohesiveness. The bonds are weak enough to allow the plates to slip past each other when the clay is being moulded, but strong enough to hold the plates in place and allow the moulded clay to retain its shape.   Source: https://en.wikipedia.org/wiki/Kaolinite

It is this slipperiness that makes it a good carrier of the aluminium hydrate. However, kaolin begins a non-reversable change from hexagonal plates to a crystalline form at about 600C/1100F and completes it by 900C/1650F. It is the crystalline form that sticks to glass. So, it is the clay (kaolin) that needs to be removed from the glass.

Hydrochloric acid as a cleaner of kiln wash

Glass is almost impervious when it has a minimum of modifiers. Glass which has a minimum amount of [modifiers] and is almost entirely SiO2 is remarkably chemically inert and reacts only with very strong alkaline (bases) materials.   Source: https://www.quora.com/How-come-hydrochloric-acid-does-not-burn-through-the-glass-bottle-that-its-stored-in

Note that coloured and fusing glass have a significant level of sodium and potassium modifiers. This means that fusing glass is subject to attack by hydrochloric acid. 

Safety notes on hydrochloric acid

Being a strong acid, hydrochloric acid is corrosive to living tissue and to many materials, but not to rubber. Typically, rubber protective gloves and related protective gear are used when handling concentrated solutions. Solutions of less than 25% cause skin irritation, serious eye irritation and respiratory irritation. Over 25% causes severe skin burns and eye damage. It is also a precursor of many illegal drugs. Serious safety gear is required to handle even 10% solutions. 

Even then:

“Clays are not truly soluble in HCl acid, [but] exposure to HCl acid does affect the structure of clay minerals. Hydrochloric acid cleans clay minerals by removing free iron oxide from the surface. … The dissolution of kaolinite clay in hydrochloric acid solutions has been carried out in the presence of fluoride ions. Leaching in the presence of fluoride ions activates the clay for leaching, making higher extractions possible at lower roasting and leaching temperatures. Acetic acid [vinegar] is less effective.”   Source: Stability of Clay Minerals in Acid, by D E Simon and M S Anderson. https://onepetro.org/SPEFD/proceedings-abstract/90FD/All-90FD/SPE-19422-MS/68436 

This piece of research shows that hydrochloric acid is most effective in combination with fluoride and heat.

Other reported research from Researchgate shows:

“Kaolin and other clays are partly soluble in acidic solutions (organic or inorganic acids in water) but the … solubility is never complete. Increasing the acid content doesn't … increase the solubility.” Philip G Jessop, Queen's University. 

       “Potassium hydroxide … will get kaolinite dissolved with a white residue for selective leaching. … The most aggressive solvent is hydrofluoric acid which "kills" almost all silicates [including kaolin]. … For the kaolinite group … use hydrazine as solvent.” Harald G. Dill, Leibniz Universität Hannover. 

Hydrazine is highly toxic unless handled in solution. Hydrofluoric acid may dissolve the kaolin, but it also dissolves the minerals in glass. Both these chemicals are extremely dangerous. 

Conclusion

It is not advisable to use hydrochloric (muriatic) acid as a cleaner of the kaolin in kiln wash from glass. 

There are other much safer methods which use a chelating action rather than attempting to dissolve the almost insoluble kaolin. These are citric acid for brief (less that 24 hours) soaking, or trisodium citrate for longer periods.