Multiple Firings of Kiln Wash

›
Many people report that they fire multiple times on kiln wash that has not been renewed.   Most add coats over existing kiln wash.   They on...
2 comments:
Wednesday, 4 October 2023

Muriatic acid as a cleaner of kiln wash

›
Muriatic acid is a common name for hydrochloric acid.      Let’s look at what is being cleaned off first. The main components of kiln wash...
Wednesday, 21 June 2023

Kiln Wash Sticking to Glass

›
Causes and avoidance   Photo credit: Immerman Glass  In general, kiln wash for glass is made up of aluminium hydrate with kaolin (China ...
Wednesday, 15 February 2023

Conditions for Re-firing Kiln Wash

›
I do not know the exact chemical changes of kiln wash at fusing temperatures.  But I do suspect it has to do with the kaolin.  The aluminium...
Wednesday, 22 December 2021

Glass Separators

›
Glass separators tend to be in three forms – powdered, liquid  or  fibre . These are applied to shelves, moulds and other surfaces that m...
Saturday, 22 December 2018

Batt Wash Sticking to the Glass

›
The main conditions in which kiln wash sticks to glass are: 1. Firing at too high a temperature. The higher the temperature, the more like...
›